inconel600 nickel-based alloy 600 chemical composition density physical properties
Inconel 600 Introduction:
Alloy 600 is a nickel-chromium-iron-based solid solution strengthened alloy. It has good high-temperature corrosion resistance and oxidation resistance, excellent hot and cold processing and welding process performance, and has satisfactory thermal strength and high plasticity below 700 degree . Alloys can be strengthened by cold working or joined by resistance welding, fusion welding or brazing.
Inconel 600 has the following features:
1. It has good resistance to corrosion by reducing, oxidizing and nitriding media.
2. It has good resistance to stress corrosion cracking at room temperature and high temperature.
3. It has good resistance to corrosion by dry chlorine gas and hydrogen chloride gas.
4. It has good mechanical properties at zero, room temperature and high temperature.
5. It has good creep rupture resistance and is recommended for use in working environments above 700 degree .


Metallographic structure of Inconel 600:
Inconel 600 has a face-centered cubic lattice structure.
Corrosion resistance of Inconel 600:
Alloy 600 is corrosion resistant to various corrosive media. The composition of chromium gives this alloy better corrosion resistance under oxidizing conditions than Nickel 99.2 (Alloy 200) and Nickel 99.2 (Alloy 201, low carbon). At the same time, the higher nickel content gives the alloy good corrosion resistance in reducing conditions and alkaline solutions, and can effectively prevent chlorine-iron stress corrosion cracking. Alloy 600 has good corrosion resistance in organic acids such as acetic acid, acetic acid, formic acid, and stearic acid, and moderate corrosion resistance in inorganic acids. It has excellent corrosion resistance in high-purity water used in primary and secondary circulation in nuclear reactors. The particularly outstanding performance of 600 is its resistance to corrosion by dry chlorine and hydrogen chloride, and the application temperature can reach 650 degree . At high temperatures, annealed and solution-treated alloys have good resistance to oxidation spalling and high strength in the air. The alloy is also resistant to ammonia gas and nitriding and carburizing atmospheres, but when the redox conditions alternate, the alloy will be corroded by partially oxidizing media (such as green death liquid)
Inconel 600 process performance and requirements:
1. Thermal processing temperature range is 1200 degree ~900 degree , and the cooling method is water quenching or rapid air cooling.
2. To obtain corrosion resistance and a very suitable crystal structure, heat treatment is required after heat processing.
3. Materials can be fed directly into the heated furnace.
1. Cold worked materials should be in an annealed or solution heat treated state. The work hardening rate of 600 alloy is close to that of austenitic stainless steel, so similar processing equipment can be selected.
2. Intermediate annealing should be performed during the cold working process.
3. When the cold working amount is greater than 5%, the workpiece needs to be solution treated.
4. To reduce material wear, the mold should be made of alloy tool steel, carbide or cast steel.
Inconel600 welding process
The alloy has good welding performance and can be connected by various methods such as arc welding, argon arc welding, resistance welding and brazing. Large or complex welded structural parts should be annealed at 870 degree for 1 hour after welding to eliminate welding stress.
Inconel600 parts heat treatment process
Inconel 600 application areas include:
1. Thermowells in corrosive atmosphere
2. Vinyl chloride monomer production: resistant to chlorine gas, hydrogen chloride, oxidation and carbonization corrosion
3. Oxidation of uranium into hexafluoride: resistant to hydrogen fluoride corrosion
4. Fields of production and use of corrosive alkali metals, especially environments where sulfides are used
5. Preparation of titanium dioxide using chlorine gas method
6. Production of organic or inorganic chlorides and fluorides: 7. Nuclear reactors
8. Retorts and components in heat treatment furnaces, especially in carbonizing and nitriding atmospheres
9. For catalytic regenerators in petrochemical production, alloy 600 is recommended for applications above 700 degree to obtain a longer service life.
Inconel600 is often used in engineering practice, which is a nickel-based solid solution strengthened high-temperature alloy. There are many difficulties in cutting this material, such as high cutting force, high cutting temperature, severe tool wear, etc. In view of these difficulties, this article proposes the reasonable selection of cutting amount, tool material, tool geometric angle and cutting fluid when processing this material.