Inconel 600 rund stang vægtdiagram, Nikkel 600 rund stang vægt pr. meter, Inconel 600 Alloy rund stang vægt diagram, 600 legering stang vægt diagram.
Inconel 600 rundstangstolerancediagram
| Dia | Vægt | Dia | Vægt |
|---|---|---|---|
| (mm) | per meter (kg) | (i) | per meter (kg) |
| 3 mm | 0.06 | 1/8″ | 0.06 |
| 4 mm | 0.10 | 3/16″ | 0.14 |
| 5 mm | 0.16 | 1/4″ | 0.25 |
| 6 mm | 0.22 | 5/16″ | 0.39 |
| 7 mm | 0.30 | 3/8″ | 0.56 |
| 8 mm | 0.40 | 7/16″ | 0.77 |
| 10 mm | 0.62 | 1/2″ | 1.00 |
| 12 mm | 0.89 | 9/16″ | 1.22 |
| 14 mm | 1.22 | 5/8″ | 1.56 |
| 15 mm | 1.40 | 11/16″ | 1.89 |
| 16 mm | 1.59 | 3/4″ | 2.25 |
| 18 mm | 2.01 | 7/8″ | 3.07 |
| 20 mm | 2.48 | 1″ | 4.03 |
| 22 mm | 3.00 | ||
| 24 mm | 3.57 | ||
| 25 mm | 3.88 |
Inconel 600 bar lagerleverandør. Nikkel 600 metrisk rundt stangvægtdiagram, 12 mm rundt stangvægtdiagram.