Dimensioner og toleranceoplysninger for 601 legeret rundstænger

Dimensioner Standard Af Inconel 601 Rundstang

Diameter el
Bredde
(mm)
Vægt pr meter Snitareal Perimeter
  Firkant
(kg)
Rund
(kg)
Firkant
(cm²)
Rund
(cm²)
Firkant
(cm)
Rund
(cm)
5.0 0.20 0.15 0.25 0.20 2.0 1.57
5.5 0.24 0.19 0.30 0.24 2.2 1.78
6.0 0.28 0.22 0.36 0.28 2.4 1.88
7.0 0.38 0.30 0.49 0.38 2.8 2.20
8.0 0.50 0.39 0.64 0.50 3.2 2.51
9.0 0.64 0.50 0.81 0.64 3.6 2.83
10 0.73 0.63 1.00 0.79 4.0 3.14
11 0.95 0.75 1.21 0.95 4.4 3.46
12 1.13 0.89 1.44 1.13 4.8 3.77
14 1.54 1.21 1.96 1.54 5.6 4.40
16 2.01 1.58 2.56 2.01 6.4 5.03
18 2.54 2.00 3.24 2.54 7.2 5.65
20 3.14 2.47 4.00 3.14 8.0 6.28
22 3.80 2.98 4.84 3.80 8.8 6.91
25 4.91 3.85 6.25 4.91 10.0 7.85
28 6.15 4.83 7.84 6.16 11.2 8.80
32 8.04 6.31 10.24 8.04 12.8 10.05
36 10.17 7.99 12.96 10.18 14.4 11.31
40 12.56 9.86 16.00 12.57 16.0 12.57
45 15.90 12.49 20.25 15.90 18.0 14.14
50 19.62 15.41 25.00 19.64 20.0 15.71
56 24.62 19.34 31.36 24.63 22.4 17.59
63 31.16 24.47 36.69 31.17 25.2 19.79
71 39.57 31.08 50.41 39.59 28.4 22.31
80 50.24 39.46 64.00 50.27 32.0 25.13

 

Inconel UNS N06601 Bright rundstangstolerance

Inconel 601 rundstangstolerance ISO "H"-serien i MM
Størrelse (mm) H12 H11 H10 H9 H8 H7 H6 H5
Over 180 - 250 +0.46/0 +0.29/0 +0.185/0 +0.115/0 +0.072/0 +0.046/0 +0.029/0 +0.02/0
Over 120 - 180 +0.4/0 +0.25/0 +0.16/0 +0.1/0 +0.063/0 +0.04/0 +0.025/0 +0.018/0
Over 80 - 120 +0.35/0 +0.22/0 +0.14/0 +0.087/0 +0.054/0 +0.035/0 +0.022/0 +0.015/0
Over 50 - 80 +0.3/0 +0.19/0 +0.12/0 +0.074/0 +0.046/0 +0.03/0 +0.019/0 +0.013/0
Over 30 - 50 +0.25/0 +0.16/0 +0.1/0 +0.062/0 +0.039/0 +0.025/0 +0.016/0 +0.011/0
Over 18 - 30 +0.21/0 +0.13/0 +0.084/0 +0.052/0 +0.033/0 +0.021/0 +0.013/0 +0.009/0
Over 10 - 18 +0.18/0 +0.11/0 +0.07/0 +0.043/0 +0.027/0 +0.018/0 +0.011/0 +0.008/0
Over 6 - 10 +0.15/0 +0.09/0 +0.058/0 +0.036/0 +0.022/0 +0.015/0 +0.009/0 +0.006/0
Over 3 - 6 +0.12/0 +0.075/0 +0.048/0 +0.03/0 +0.018/0 +0.012/0 +0.008/0 +0.005/0
~ til 3 +0.1/0 +0.06/0 +0.04/0 +0.025/0 +0.014/0 +0.01/0 +0.006/0 +0.004/0

 